Re: Patillo's glass tube


Jim Patillo
 

Dennis,

I presumed Ron knew to use Bondo or some other filling material with
release agent after getting the shape prior to glass. I guess I
should have been more clear. Sanding was just to knock off any
residue.

I actually made a quick disconnect aux tank using a foam shape then
Bondo and a release agent which was written up long ago.

Thanks for the clarification.

JP

--- In Q-LIST@..., denpau@m... wrote:
Shape your foam tube, cover with wall joint
compound, sand smooth, paint with water
base paint, spray with release agent.
The release agent will ruin the joint
compound if not painted. Allow to dry,
then glass.
When cured, pour gas inside, pull out
the waste.
The inside of the tube will be
smoother than the outside.

Dennis Clark
N4324S